XRD patterns XRD patterns of

These results indicate birth rate homogeneous glass sample could be prepared in xNCFAS system when ‘x’ is less than 13.
Fig. 3. XRD patterns of 15Na2O⋅15CaO⋅40Fe2O3⋅xAl2O3⋅(30−x)SiO2 samples with ‘x’ of (a) 0, (b) 5, (c) 10, (d) 15 and (e) 20; those recorded before (A) and after (B) annealing at 1000 °C for 100 min.Figure optionsDownload full-size imageDownload as PowerPoint slide