In addition, supported Ni catalyst on activated carbon (AC) with the Ni loading of 7.2 wt.% was prepared by incipient wetness impregnation using nickel nitrate aqueous solution. The slurry was dried at 80 °C overnight and calcined at 350 °C for 2 h in air. Finally, the solid was reduced under 10% v/v H2/Ar at 500 °C for 2 h with a ramping rate of 5 °C/min. The obtained sample was referred to as IM-Ni/AC.